Join our Premium Membership now and save with Xpres, Listawood, Ink Experts, Ink Express and more! Just £10 per year.....Click the Membership link above.....

User Tag List

Similar Threads

  1. Chromaluxe sublimation help
    By bross1004 in forum General Dye-Sub Chit Chat
    Replies: 6
    Last Post: 01-11-2018, 07:24 AM
  2. Chromaluxe chipping
    By GoonerGary in forum Printing Problems/Issues
    Replies: 18
    Last Post: 24-05-2018, 08:44 AM
  3. Pet Tags - Problem with edges chipping/wearing within 1-2 days
    By tjt in forum Printing Problems/Issues
    Replies: 2
    Last Post: 26-04-2017, 08:49 PM
  4. Chipping Issues - small id tags
    By SrPerro in forum Printing Problems/Issues
    Replies: 3
    Last Post: 29-04-2012, 10:13 AM
  5. Chromaluxe panels
    By fredster in forum Sourcing New Items
    Replies: 3
    Last Post: 20-09-2010, 03:31 AM
Results 1 to 7 of 7
  1. #1
    Member
    Join Date
    May 2019
    Location
    Southampton
    Posts
    29
    Downloads
    0
    Uploads
    0
    Mentioned
    0 Post(s)
    Tagged
    0 Thread(s)

    Chromaluxe chipping?

    Hi all. Any help much appreciated. Just sublimated my first aluminium picture and all was good except a slight chip on one corner. Have a got the pressure on too much?

    I used the pressing guide so 3.04 secs. 7 or 8 pressure at 195c. I used Teflon under sheet, then paper then image with aluminium on top covered by the fabric they advise to use.

    loving it so far just need to sort out that imperfection!

    best wishes and many thanx in advance to any help. Claire :)
    Attached Images Attached Images

  2. #2
    Member
    Join Date
    May 2019
    Location
    Southampton
    Posts
    29
    Downloads
    0
    Uploads
    0
    Mentioned
    0 Post(s)
    Tagged
    0 Thread(s)
    Chip is in bottom left corner. Tried to load a second pic but iPad playing up! Lol ��

  3. #3
    Senior Member
    Join Date
    Jun 2010
    Location
    Cambridge
    Posts
    2,369
    Downloads
    0
    Uploads
    0
    Mentioned
    4 Post(s)
    Tagged
    1 Thread(s)
    It chips. The EU banned a chemical which was used for bonding the coating.

    https://www.dyesubforum.co.uk/vbforu...ght=chromaluxe

  4. #4
    Member
    Join Date
    May 2019
    Location
    Southampton
    Posts
    29
    Downloads
    0
    Uploads
    0
    Mentioned
    0 Post(s)
    Tagged
    0 Thread(s)
    Thanx for that Gary. The plastic coat pulled away fine. I didnt check it before using though! Maybe it was already damaged? Will try again with some more images. Luckily this is for me but I did want to sell them for others.

    Many thanx for your time and info. Best wishes Claire :)

  5. #5
    Senior Member
    Join Date
    Jun 2010
    Location
    Cambridge
    Posts
    2,369
    Downloads
    0
    Uploads
    0
    Mentioned
    4 Post(s)
    Tagged
    1 Thread(s)
    Where did you buy the Chromaluxe sheets from?

  6. #6
    Member
    Join Date
    May 2019
    Location
    Southampton
    Posts
    29
    Downloads
    0
    Uploads
    0
    Mentioned
    0 Post(s)
    Tagged
    0 Thread(s)
    I bought it from Xpres. They were very helpful; so today I’m going to follow up on the threads advice of talking to Chromaluxe and Xpres if I get no joy.

  7. #7
    Senior Member
    Join Date
    Jun 2010
    Location
    Cambridge
    Posts
    2,369
    Downloads
    0
    Uploads
    0
    Mentioned
    4 Post(s)
    Tagged
    1 Thread(s)
    My sheets were also from Xpres, but I'm guessing that all new EU stock is rubbish.